Re, Rhenium

bar

RHENIUM S E 4d7/2 4d5/2 Ref.
Re 8 1 40.46 260.5 79-20
ReO2 3 1 43.2   83-11
Re2O7     46.7   80-3
K2ReO4     46.07   85-13
NH4ReO4     46.2   83-11
NBu4ReO4     44.67   85-13
ReOCl3(PPh3)2     43.7   73-4
K2ReBr6     43.5   80-22
K2ReCl6 3   44.0   80-22
ReCl4(PEt3)2     433   72-5
 

bar

 
Notes
S Number of independent studies (where this is greater than 1)
E Number of these rejected as unsound (mainly early measurements) before the remaining ones were used to determine a mean value
A.P Auger parameter (calculated from the most intense photoelectron line and Auger line)
M.A.P. Modified Auger Parameter
v Referenced to the vacuum level (gases)
c Includes minor corrections in high binding energy lines using X-ray energy data from reference 67-1
Refs. Reference in which the data was originally published. (See the references section)
  

bar

bar

Navigation Bar Navigation Bar

bar

Last updated 24 February, 2001

Compiled by and
Christopher Walker
KLA-Tencor,
686 Stirling Road
Slough
Berks., UK
Simon Morton
Advanced Light Source
Lawrence Berkeley Laboratory
Berkeley
CA 94720
email chris.walker@physics.org email S.Morton@uksaf.org

bar
© UK Surface Analysis Forum 1998