TITANIUM S E 2p3/2 L3M23V A.P. Ref.
Ti     453.89     81-9
Ti 5   454.0 419.0 873.0 79-18
TiP     454.8     85-10
TiN     455.8     76-16
TiC     454.6 418.2 872.8 79-17
TiO2 10 2 458.7     79-18
TiO acetylacetonate     458.4 414.8 873.2 79-17
Titanocene dichloride     457.2 414.9 872.1 79- 17
TiCl4     458.5     83-15
BaTiO3 2   458.55     75-10
Na2TiF6     462.6 409.8 872.4 79- 17
K2TiF6     462.1 409.4 871.5 79-17
 

bar

 
Notes
S Number of independent studies (where this is greater than 1)
E Number of these rejected as unsound (mainly early measurements) before the remaining ones were used to determine a mean value
A.P Auger parameter (calculated from the most intense photoelectron line and Auger line)
M.A.P. Modified Auger Parameter
v Referenced to the vacuum level (gases)
c Includes minor corrections in high binding energy lines using X-ray energy data from reference 67-1
Refs. Reference in which the data was originally published. (See the references section)
  

bar

bar

Navigation Bar Navigation Bar

bar

Last updated 24 February, 2001

Compiled by and
Christopher Walker
KLA-Tencor,
686 Stirling Road
Slough
Berks., UK
Simon Morton
Advanced Light Source
Lawrence Berkeley Laboratory
Berkeley
CA 94720
email chris.walker@physics.org email S.Morton@uksaf.org

bar
© UK Surface Analysis Forum 1998