Zn, Zinc

bar

ZINC S E 2p3/2 L3M45M45 A.P. Ref.
Zn     1021 82     81- 9
Zn 13 2 1021.70 992.10 2013.80 85-4
ZnP2     1020.9     75- 12
ZnTe     1021.6c 991.3 2012.9c 77-12
ZnSe     1022.0c 989.5 2011.5c 77-12
ZnS 3   1021.6c 989.7 2011.3c 77-11
ZnO 11 2 1022.1c 987.7 2009.8c 77-11
ZnI2 2   1022.5c 988.7 2011.2c 77-11
ZnBr2 2   1023.4 987.3 2010.7 75-14
ZnCl2         2009.2c 77- 12
ZnAl2O4     1021.7 987.8 2009.5 84-22
ZnSO4 2   1023.0 986.2 2009.2 84-22
ZnF2 2   1021.8c 986.2 2008.0c 77-11
Zn(g)       974.5v   77- 3
 

bar

 
Notes
S Number of independent studies (where this is greater than 1)
E Number of these rejected as unsound (mainly early measurements) before the remaining ones were used to determine a mean value
A.P Auger parameter (calculated from the most intense photoelectron line and Auger line)
M.A.P. Modified Auger Parameter
v Referenced to the vacuum level (gases)
c Includes minor corrections in high binding energy lines using X-ray energy data from reference 67-1
Refs. Reference in which the data was originally published. (See the references section)
  

bar

bar

Navigation Bar Navigation Bar

bar

Last updated 24 February, 2001

Compiled by and
Christopher Walker
KLA-Tencor,
686 Stirling Road
Slough
Berks., UK
Simon Morton
Advanced Light Source
Lawrence Berkeley Laboratory
Berkeley
CA 94720
email chris.walker@physics.org email S.Morton@uksaf.org

bar
© UK Surface Analysis Forum 1998